Cheap Chemically Cross-linked PE closed cell Foam - Foam-010
Material: PE | Type: Foam | Place of Origin: Jiangsu China (Mainland) | Brand Name: Hanata |
Model Number: Foam-010 | Density: 30-200 | Width: 60-180cm | Thickness: 3mm-250mm |
Color: All |

Feature: CUSHION and SHRINK & RISE MATERIAL Physical Properties of XPE Foam | ||||||||
Testing Item | Properties | |||||||
5 times | 8times | 10times | 15times | 20times | 25times | 30times | 35times | |
Density kg/m3 | 200±30 | 125±15 | 100±10 | 66.7±8 | 50±6 | 40±4 | 33.3±3 | 28.6±2 |
Shore Hardness ° | 60~70 | 50~60 | 45~50 | 35~45 | 30~35 | 25~30 | 18~25 | 13~18 |
Water Absortion Rate (23°C±,24h)g/cm2 | ≤0.02 | ≤0.02 | ≤0.03 | ≤0.03 | ≤0.04 | ≤0.04 | ≤0.05 | ≤0.05 |
Thermal conductivity (W/m.k) | ≤0.092 | ≤0.082 | ≤0.072 | ≤0.062 | ≤0.053 | ≤0.047 | ≤0.041 | ≤0.038 |
Tensile Strength (L/W)MPa | ≥1.35/1.08 | ≥1.12/0.89 | ≥0.88/0.71 | ≥0.68/0.56 | ≥0.39/0.33 | ≥0.33/0.25 | ≥0.25/0.20 | ≥0.20/0.16 |
Tensibility(L/W)% | ≥260/220 | ≥230/200 | ≥210/185 | ≥190/170 | ≥170/150 | ≥160/135 | ≥140/130 | ≥120/110 |
tearing strength(L/W)kN/m | ≥5.90/7.10 | ≥4.80/5.40 | ≥3.60/4.00 | ≥2.80/3.30 | ≥1.80/2.30 | ≥1.60/2.00 | ≥1.35/1.70 | ≥1.25/1.50 |
compression set (25%,22h)% | ≤5 | ≤6 | ≤7 | ≤7 | ≤9 | ≤9 | ≤11 | ≤11 |
Dimensional Change rate (70±,22h)(L/W)% | ≤-6/-4 | ≤-6/-4 | ≤-6/-4 | ≤-6/-4 | ≤-6/-4 | ≤-8/-6 | ≤-8/-6 | ≤-8/-6 |